Purifying?agent?for?molten?zinc?in?HDG
Name:
Purifying?agent?for?molten?zinc?in?HDG
  • Model:
  • Uses:
  •  
Details

In the light of the high iron and impurity contents in molten zinc, poor fluidness and particles and fold on workpiece often occurred in hot galvanizing plants, our company has organized the famous specialists and scientific and technological personnel in many disciplines at home developed XY-XG-3 type purifying agent for molten zinc, a high and new technical product. It has effectively solved the difficult problem and filled in the gap in this field at home. Through testing and using, the agent reached the anticipated results and is well received by customers. At present the product is applying for a patent. 
Notice
Do well pretreatment work, do not carry the harmful impurity into zinc pot, galvanizing agent needs the acid and iron eliminating, and it would be best if rinsing water for pretreatment could be fluid.
Because of the high volatility of the agent, No.2 operation should be quickly performed.
In order to avoid the splashing of molten zinc causing danger, operators should be well dressed in labor protection articles. Operation with caution and safety first.
Purifying Treatment Method of Molten Zinc:
Keep furnace temperature at 450℃-470℃.
Place dry thermal insulation bricks (with strong water absorption) into box with holes, quickly pour the purifying agent to them, insert the box into molten zinc and move it back and forth until boiling ends, and take out the box with holes.
Eliminate suspended substances on the surface of molten zinc; scatter ammonium chloride (1-1.5 kg/ m2) to further eliminate impurity on the surface.
Repeat the abovementioned steps three or four times.
Add the alloy, which is 0.5% of molten zinc, in uniform distribution way. After all the melting, repeat the abovementioned step once. (If there are excessive aluminum or other alloys in original molten zinc, the step-by-step method can be used)
The temperature is controlled at 430℃-440℃ and the standing time is 6-12 h (time is as long as possible).
When small workpiece is tested (the temperature is at 430℃ and dipping time is not changed), the surface and coating thickness is measured. If the coating is thick, the alloy, which is 0.1 % of molten zinc, can be added. 
The zinc and the alloy can be added at one time until the alloy content in molten zinc reaches 1.5%.
After alloying is completed, the working temperature of molten zinc should be controlled at 440℃±5℃ and the lifting speed of traveling crane at 1.5 m / min.
 

 

返回頂部 電話
主站蜘蛛池模板: 亚洲v无码专区在线亚 | 一区久久影视 | 国产欧美日韩综合精品一区二区 | v无码精品一区二区在线观看 | 久久综合婷婷丁香五月中文字幕 | 国产成人精品一区二区三区不卡 | 国产高清在线视频大 | 亚洲国精产 | 高清日韩国产无码一区二区 | 日韩精品无码专 | 欧美成人全部费免网站 | 亚洲精品天天 | 亚洲国产中文成人久久综合 | 精品动漫一区二区无码视频 | 国产寡妇xxxx猛交巴巴 | 国产精品精品二区 | 国产末成年av女在线播放 | 2025av在线无码 | 国产大学生a片视频播放 | 亚洲导航深夜福利 | 亚洲熟妇av一区二区三区 | 又大又紧又粉嫩18p少妇 | 日本欧美真人三级在线a | 国产在线麻豆精 | 欧美国产日韩极速在线 | 日韩视频中文字幕专区 | 国产91久久九九免费精品无码 | 91久久夜色精品国产网站 | 日韩欧美在线播放 | 一区二区欧美日韩高清免费 | 亚洲国产成人精品区综合 | 日本韩国野花视频爽国产在线 | 99久久无码热高 | 朝桐光一区二区 | 午夜激情经典五月天影院 | av无码免费久久久精品 | 欧美综合自拍亚洲综合图片区 | 综合无码一区二区三区四区五区 | 亚洲精品99久久久久中文字幕 | 亚洲欧美国产国产一区二区 | 丰满少妇在线 |